  <dc:description xmlns:ns0="xml" ns0:lang="en">OBJECTIVE
To assess the 5-year survival of metal-ceramic and all-ceramic tooth-supported single crowns (SCs) and to describe the incidence of biological, technical and esthetic complications.


METHODS
Medline (PubMed), Embase, Cochrane Central Register of Controlled Trials (CENTRAL) searches (2006-2013) were performed for clinical studies focusing on tooth-supported fixed dental prostheses (FDPs) with a mean follow-up of at least 3 years. This was complimented by an additional hand search and the inclusion of 34 studies from a previous systematic review [1,2]. Survival and complication rates were analyzed using robust Poisson's regression models to obtain summary estimates of 5-year proportions.


RESULTS
Sixty-seven studies reporting on 4663 metal-ceramic and 9434 all-ceramic SCs fulfilled the inclusion criteria. Seventeen studies reported on metal-ceramic crowns, and 54 studies reported on all-ceramic crowns. Meta-analysis of the included studies indicated an estimated survival rate of metal-ceramic SCs of 94.7% (95% CI: 94.1-96.9%) after 5 years. This was similar to the estimated 5-year survival rate of leucit or lithium-disilicate reinforced glass ceramic SCs (96.6%; 95% CI: 94.9-96.7%), of glass infiltrated alumina SCs (94.6%; 95% CI: 92.7-96%) and densely sintered alumina and zirconia SCs (96%; 95% CI: 93.8-97.5%; 92.1%; 95% CI: 82.8-95.6%). In contrast, the 5-year survival rates of feldspathic/silica-based ceramic crowns were lower (p&lt;0.001). When the outcomes in anterior and posterior regions were compared feldspathic/silica-based ceramic and zirconia crowns exhibited significantly lower survival rates in the posterior region (p&lt;0.0001), the other crown types performed similarly. Densely sintered zirconia SCs were more frequently lost due to veneering ceramic fractures than metal-ceramic SCs (p&lt;0.001), and had significantly more loss of retention (p&lt;0.001). In total higher 5 year rates of framework fracture were reported for the all-ceramic SCs than for metal-ceramic SCs.


CONCLUSIONS
Survival rates of most types of all-ceramic SCs were similar to those reported for metal-ceramic SCs, both in anterior and posterior regions. Weaker feldspathic/silica-based ceramics should be limited to applications in the anterior region. Zirconia-based SCs should not be considered as primary option due to their high incidence of technical problems.</dc:description>
  <dc:format>application/pdf</dc:format>
  <dc:identifier>https://sonar.ch/global/documents/140346</dc:identifier>
  <dc:language>eng</dc:language>
  <dc:relation>info:eu-repo/semantics/altIdentifier/doi/10.1016/j.dental.2015.02.011</dc:relation>
  <dc:relation>info:eu-repo/semantics/altIdentifier/pmid/25842099</dc:relation>
  <dc:rights>info:eu-repo/semantics/openAccess</dc:rights>
  <dc:source>Dental materials : official publication of the Academy of Dental Materials. - 2015</dc:source>
  <dc:subject xmlns:ns1="xml" ns1:lang="en">All-ceramic</dc:subject>
  <dc:subject xmlns:ns2="xml" ns2:lang="en">Biological complications</dc:subject>
  <dc:subject xmlns:ns3="xml" ns3:lang="en">Complication rates</dc:subject>
  <dc:subject xmlns:ns4="xml" ns4:lang="en">Failures</dc:subject>
  <dc:subject xmlns:ns5="xml" ns5:lang="en">Longitudinal</dc:subject>
  <dc:subject xmlns:ns6="xml" ns6:lang="en">Single crowns</dc:subject>
  <dc:subject xmlns:ns7="xml" ns7:lang="en">Success</dc:subject>
  <dc:subject xmlns:ns8="xml" ns8:lang="en">Survival</dc:subject>
  <dc:subject xmlns:ns9="xml" ns9:lang="en">Systematic review</dc:subject>
  <dc:subject xmlns:ns10="xml" ns10:lang="en">Technical complications</dc:subject>
  <dc:subject xmlns:ns11="xml" ns11:lang="en">Ceramics</dc:subject>
  <dc:subject xmlns:ns12="xml" ns12:lang="en">Crowns</dc:subject>
  <dc:subject xmlns:ns13="xml" ns13:lang="en">Dental Prosthesis Design</dc:subject>
  <dc:subject xmlns:ns14="xml" ns14:lang="en">Dental Prosthesis, Implant-Supported</dc:subject>
  <dc:subject xmlns:ns15="xml" ns15:lang="en">Dental Restoration Failure</dc:subject>
  <dc:subject xmlns:ns16="xml" ns16:lang="en">Esthetics, Dental</dc:subject>
  <dc:subject xmlns:ns17="xml" ns17:lang="en">Humans</dc:subject>
  <dc:subject xmlns:ns18="xml" ns18:lang="en">Metal Ceramic Alloys</dc:subject>
  <dc:subject xmlns:ns19="xml" ns19:lang="en">Metals</dc:subject>
  <dc:title xmlns:ns20="xml" ns20:lang="en">All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part I: Single crowns (SCs).</dc:title>