  <dc:creator>Stawarczyk B</dc:creator>
  <dc:creator>Hartmann L</dc:creator>
  <dc:creator>Hartmann R</dc:creator>
  <dc:creator>Roos M</dc:creator>
  <dc:creator>Ender A</dc:creator>
  <dc:creator>Ozcan M</dc:creator>
  <dc:creator>Sailer I</dc:creator>
  <dc:creator>Hämmerle CH</dc:creator>
  <dc:date>2012</dc:date>
  <dc:description xmlns:ns0="xml" ns0:lang="en">This study tested the impact of Gluma Desensitizer on the tensile strength of zirconia crowns bonded to dentin. Human teeth were prepared and randomly divided into six groups (N = 144, n = 24 per group). For each tooth, a zirconia crown was manufactured. The zirconia crowns were cemented with: (1) Panavia21 (PAN), (2) Panavia21 combined with Gluma Desensitizer (PAN-G), (3) RelyX Unicem (RXU), (4) RelyX Unicem combined with Gluma Desensitizer (RXU-G), (5) G-Cem (GCM) and (6) G-Cem combined with Gluma Desensitizer (GCM-G). The initial tensile strength was measured in half (n = 12) of each group and the other half (n = 12) subjected to a chewing machine (1.2 Mio, 49 N, 5°C/50°C). The cemented crowns were pulled in a Universal Testing Machine (1 mm/min, Zwick Z010) until failure occurred and tensile strength was calculated. Data were analyzed with one-way and two-way ANOVA followed by a post hoc Scheffé test, t test and Kaplan-Meier analysis with a Breslow-Gehan analysis test (α = 0.05). After the chewing simulation, the self-adhesive resin cements combined with Gluma Desensitizer showed significantly higher tensile strength (RXU-G, 12.8 ± 4.3 MPa; GCM-G, 13.4 ± 6.2 MPa) than PAN (7.3 ± 1.7 MPa) and PAN-G (0.9 ± 0.6). Within the groups, PAN, PAN-G and RXU resulted in significantly lower values when compared to the initial tensile strength; the values of all other test groups were stable. In this study, self-adhesive resin cements combined with Gluma Desensitizer reached better long-term stability compared to PAN and PAN-G after chewing simulation.</dc:description>
  <dc:format>application/pdf</dc:format>
  <dc:identifier>https://sonar.ch/global/documents/165729</dc:identifier>
  <dc:language>eng</dc:language>
  <dc:relation>info:eu-repo/semantics/altIdentifier/doi/10.1007/s00784-010-0502-y</dc:relation>
  <dc:relation>info:eu-repo/semantics/altIdentifier/pmid/21336631</dc:relation>
  <dc:rights>info:eu-repo/semantics/openAccess</dc:rights>
  <dc:source>Clinical oral investigations. - 2012</dc:source>
  <dc:subject xmlns:ns1="xml" ns1:lang="en">Bite Force</dc:subject>
  <dc:subject xmlns:ns2="xml" ns2:lang="en">Cementation</dc:subject>
  <dc:subject xmlns:ns3="xml" ns3:lang="en">Crowns</dc:subject>
  <dc:subject xmlns:ns4="xml" ns4:lang="en">Dental Bonding</dc:subject>
  <dc:subject xmlns:ns5="xml" ns5:lang="en">Dental Cements</dc:subject>
  <dc:subject xmlns:ns6="xml" ns6:lang="en">Dental Materials</dc:subject>
  <dc:subject xmlns:ns7="xml" ns7:lang="en">Dental Restoration Failure</dc:subject>
  <dc:subject xmlns:ns8="xml" ns8:lang="en">Dental Stress Analysis</dc:subject>
  <dc:subject xmlns:ns9="xml" ns9:lang="en">Dentin</dc:subject>
  <dc:subject xmlns:ns10="xml" ns10:lang="en">Dentin Desensitizing Agents</dc:subject>
  <dc:subject xmlns:ns11="xml" ns11:lang="en">Dentin-Bonding Agents</dc:subject>
  <dc:subject xmlns:ns12="xml" ns12:lang="en">Glutaral</dc:subject>
  <dc:subject xmlns:ns13="xml" ns13:lang="en">Humans</dc:subject>
  <dc:subject xmlns:ns14="xml" ns14:lang="en">Materials Testing</dc:subject>
  <dc:subject xmlns:ns15="xml" ns15:lang="en">Methacrylates</dc:subject>
  <dc:subject xmlns:ns16="xml" ns16:lang="en">Microscopy, Electron, Scanning</dc:subject>
  <dc:subject xmlns:ns17="xml" ns17:lang="en">Phosphates</dc:subject>
  <dc:subject xmlns:ns18="xml" ns18:lang="en">Resin Cements</dc:subject>
  <dc:subject xmlns:ns19="xml" ns19:lang="en">Stress, Mechanical</dc:subject>
  <dc:subject xmlns:ns20="xml" ns20:lang="en">Temperature</dc:subject>
  <dc:subject xmlns:ns21="xml" ns21:lang="en">Tensile Strength</dc:subject>
  <dc:subject xmlns:ns22="xml" ns22:lang="en">Time Factors</dc:subject>
  <dc:subject xmlns:ns23="xml" ns23:lang="en">Zirconium</dc:subject>
  <dc:title xmlns:ns24="xml" ns24:lang="en">Impact of Gluma Desensitizer on the tensile strength of zirconia crowns bonded to dentin: an in vitro study.</dc:title>
  <dc:type>http://purl.org/coar/resource_type/c_6501</dc:type>
</oai_dc:dc>